Surface Preparation:
The covering job can only be as good as the finish of the surface it's
applied over. In order for the covering to properly adhere to a surface, the surface
must first be smooth and clean. Sand the model using a sanding block and
progressively finer sandpaper, with the final sanding being done with 320 grit
paper. Vacuum away all of the dust, as specks of dust under the covering will leave
unsightly bumps. Fill gaps and dents with a high-quality filler. If using
light-colored UltraCote® (such as white or yellow), use a tan-colored filler that
matches the wood color to prevent the filler from showing through.
|
Pro Tip
-
Some professional builders “raise the
grain” then sand a second time with 320 or 400 grit paper for the ultimate finish. After
the model is sanded, use a damp cloth to wipe down the model. Some modelers prefer to
use a fine-mist squirt bottle filled with water to dampen the surfaces to be covered. As
the surface dries, imbedded wood fibers in the surface will “stand up.” When dry, sand
the surfaces again using 320 or 400 grit paper. Raising the grain now and sanding it off
will prevent the grain from raising later under the covering, creating a bumpy finish.
Vacuum the model thoroughly and avoid touching the model with oily hands.Your model is
now ready for covering!
|
|
Trim Film to Size:
Start by covering the bottom of one wing
half. Using scissors or sharp hobby knife, cut a piece of UltraCote® a few inches larger
than needed to cover the wing. Remove the backing (save for later) and place the
covering with the adhesive (dull) side down, centered over the wing. Set the covering
iron to the application temperature of 220°F.
|
Pro Tip
- If the iron you're using does
not display the actual temperature, here is a tip that will ensure your iron is
properly set.Water boils at 212°F. Allow your iron to warm up at a medium setting.
When the iron reaches its stabilized temperature, carefully pour a few drops of
water on the iron's surface. Adjust the temperature until the water just begins to
boil off. This method is surprisingly accurate and is generally within 10° (of the
exact application temperature of 220).
|
|
Tacking Covering to Spar:
Tack the covering to the spar or the high
point of the wing, using your iron as shown (an iron sock is highly recommened). Gently
pull the covering toward the root and toward the tip, as you work the iron from the
center of the spar to the root and tip of the wing. Press gently with the iron, allowing
the heat (not pressure) to activate the adhesive and bond the covering to the high
point. Ideally, the covering will naturally lay flat against the entire surface with a
minimum of wrinkles.
|
|
Covering a Solid-Sheeted Wing:
If covering a solid-sheeted wing, work from the center of the spar
outward to the trailing edge and then to the leading edge as shown, using the iron
at 220°F. If a wrinkle develops, the covering can be carefully lifted and reapplied.
|
|
Covering an Open-Structure Wing:
If covering an open-structure wing, work from the spar toward the
trailing edge, gently sliding the iron (set at 220°) toward the trailing edge with
the iron contacting two ribs. Using your iron, adhere the covering to the remaining
ribs, working toward the tip and the root. Now complete the open structure leading
edge, using the same method. If the leading edge is sheeted, then follow the
technique listed above under “Covering a Solid-Sheeted Wing.”
|
|
Sealing the Edges:
With the iron set to 220°F, seal the leading and trailing edges. Using a
straight edge and a sharp #11 hobby knife, carefully trim the excess covering from
the leading and trailing edge, allowing a minimum of a 1/4" overlap to wrap around
the leading and trailing edge of the wing. Now seal the leading and trailing edges
securely with the covering iron.
|
|
Wing Tip:
Depending on the amount of the curvature of the wing tip, high heat (up
to 350°F) may be needed to shrink and stretch the covering to eliminate all the
wrinkles. Preset the iron to 300°F. Pull and stretch the covering around the wing
tip while applying heat with the iron. Remember, UltraCote® can be carefully lifted
and repositioned to help eliminate wrinkles. This feature is beneficial, especially
when covering sharply curved wing tips. Continue working, pulling, and heating the
covering around the tip until the covering is past the center of the tip. It may be
necessary to increase the temperature of the iron to achieve greater shrinkage to
eliminate all wrinkles. Trim the excess covering using a #11 hobby knife, then
reseal the covering on the wing tip
.
|
Pro Tip -
If sealing the covering in tight areas such as corners or fillets, using
the Hangar 9® ProTrim Sealing Tool is very helpful and results in a professional
finish.
|
|
Covering the Top of the Wing:
Using the backing from the wing panel that you just covered as a
template, cut a piece of UltraCote® to be applied to the top of the wing. Be sure to
cut a top panel, making sure that the adhesive is on the correct side. Apply the
covering to the top of the wing using the same techniques as described in steps 3
through 6. Be sure that the covering overlaps a minimum of a 1/4" when trimming the
edges and securely seal the edges with the iron.
|
|
Shrinking the Covering:
Now it’s time to shrink the covering. With the iron set to 300°F, apply
heat using the same pattern used to apply the covering starting at the spar and
working outward. It may be necessary to increase the temperature to 320°F to get rid
of stubborn wrinkles. Use the minimum amount of heat necessary to tighten the
covering.
|
Pro Tip -
Use heat, not pressure, to shrink the covering taught. If pressure is
applied, gouges can be pressed into the wood. Let heat, not pressure, do the work.
Alternate Method:
A heat gun can also be used to shrink the covering. This works
particularly well over an open structure. It can also be used over a solid structure
if a Hangar 9 Covering Glove™ is used to gently press the covering to the surface
after heat is applied.
|
|
Covering Fuselages and Other Solid Surfaces:
The technique for covering fuselages and other simple flat surfaces is
identical to covering a solid wing. Start with the bottom, then sides, and finally
the top. First, tack the center of the surface down using an iron set to 220°F. Work
outward from the center, bonding the covering to the surface. Trim and seal the
edges. About 1/4" or more overlap is recommended when applying the next piece of
covering. Shrink the covering, using the same method as described above.
|
Important:
Even if you're experienced in applying other brands of covering, it’s
important to read the following instructions. UltraCote® incorporates a unique multi
temperature controlled adhesive and shrinkage system that makes achieving
professional covering results easy.
|
Multi-Temperature Control
System:
Understanding the benefits of this system and how to use it will make
covering with UltraCote® easy and help to ensure professional results. When using
UltraCote®, there are three important temperatures to be aware of.
Application Tempature-220°F
(100°C):
At 220°, the adhesive on UltraCote® becomes active, allowing the
covering to be attached to the model.While 220° will fully bond the covering to
the model, it is well below the temperature that causes UltraCote® to shrink.
This is exactly what's needed when first attaching covering to the model to
prevent the covering from distorting.
|
Pro Tip -
Many professional builders mark this temperature on their covering
iron with a marker or striping tape for quick reference, as this temperature is
used frequently whenever putting on covering.
|
Shrink On-Set Temperature-300°F
(134°C)
At 300°F, UltraCote® begins to shrink. This is called the Shrink
On-Set point. After the covering is attached using an iron set to 220°F, the
next step is to shrink the covering. This initial shrinking is done with the
iron set at 300°F.
Maximum Shrinkage Temperature-350°F (162°C)
At 350°F, UltraCote® reaches its maximum shrinking point. Raising the
temperature above this point will not cause further shrinkage.
|
The rate of shrinkage is not
directly in proportion to the temperature. The chart to the right shows how
the majority of the shrinkage rate occurs between 300°F and 330°F. At higher
temperatures UltraCote® continues to shrink but at a much slower rate. The
smallest amount of shrinkage occurs between 340°F and 350°F. This is helpful
to remember when shrinking and tightening covering.
|
|
|
Important:
Once UltraCote® is shrunk to a specific temperature, a higher
temperature must be used to further shrink the covering. For example, if the
covering was shrunk using 320°F and wrinkles begin to appear/reappear, it will be
necessary to use over 320°F to achieve further shrinkage.
|
Pro Tip -
Always use the minimum heat necessary to remove wrinkles when tightening
the covering, thus allowing plenty of shrinkage/temperature range remaining if it's
necessary to further shrink the covering.
|
|
Helpful Hints
|
Multiple Colors:
When applying covering with a second color, it’s important that the light
color be applied first (under the dark color) to prevent the dark color from showing
through. Where colors meet or at the edge of the covering, it is important to not
overheat this area (over 300°F), as this will shrink and distort the straight edge.
Use a Sealing Iron Sock:
A covering sock placed over the iron is highly recommended, as it usually
prevents the surface of the iron from scratching. The sock absorbs heat and will
require the user to work slower or to turn the heat up 10%. Almost all professional
builders use covering socks. Hangar 9 offers one of the best that features muslin on
one side to prevent heat damage and soft cotton on the other side for a soft,
scratch-free finish. Dryer is Better:
Wood naturally absorbs moisture.Wood models actually grow and shrink
slightly throughout different seasons. This can be experienced by traveling from the
humid Midwest of the United State to the dry deserts of Las Vegas. After a few days
in the desert, the model develops covering sags due to model shrinkage. It is
recommend that you cover the model in a dry climate if possible. Placing the model
in a room with a dehumidifier for several days before covering the model may prevent
the covering from sagging due to model shrinkage.
Painting:
UltraCote® will accept most types of polyurethane, epoxy, and automotive
acrylic paints. It’s recommended that the surface be scuffed with 000 steel wool or
Scotch® bright pads then thoroughly cleaned with acetone or thinner before painting.
Model Dope or butyrate-based paint are not compatible with UltraCote®.
Bubbles and Blemishes:
Occasionally the intense heat from the sun can cause bubbles and
blemishes in the covering, especially when using dark colors. To remove these, heat
the bubbled area using a heat gun to expand the air under the covering, causing the
bubble to rise. Quickly pop the bubble using a needle then wipe the area using a
cold, wet wash cloth. The wet wash cloth rapidly cools the area, allowing the
covering to re-adhere. It may take several tries to completely remove the
bubble/blemish, but this method works great. Clean
Up:
The adhesive can be removed from the iron or model using acetone or a
mild thinner.
|
|